GRAE-P800-Flexcoat series

FLEXCOAT-GOLD-NOCON

Water agitation nonflammable,
flame retardant interior and exterior wall finishing material

Product overview

– The Graphex Coat series is a powder product modified from dry beet liquid finish
– State-of-the-art eco-friendly finishing material that reinforces the shortcomings of the existing liquid agitated dry bit finish
– New concept building interior and exterior materials made of special acrylic resin, lightweight aggregate, and various minerals

Product Features

As an interior and exterior material, it has high elasticity and is strong against crack resistance of walls 
Excellent contamination resistance, fire resistance, breathability, heat insulation, waterproofness, and adhesion
Can be used in various structures such as wooden houses and panel steel structures

Physical properties

categoryContentRemark
Main componentPorous ceramic,
highly elastic acrylic emulsion
TypeHydrophilic
Solid content70~75%
specific gravity0.7
PH6.8~7.0
Theoretical Coating Thickness1.3m²/L
ShapeOne component
Volume solids70+/-3%
Dry film thickness0.4~ 0.6mm or more
Color / Paint appearanceWhite / matte, semi-gloss

Test result

Test ItemsunitSample
classification
ResultTest Methods
Low temperature stability--clearKS F 4715 : 2007
Crack resistance according to initial drying--clearKS F 4715 : 2007
Adhesion strength (standard condition)N/㎟-0.8KS F 4715 : 2007
Adhesion strength (after immersion)N/㎟-0.6KS F 4715 : 2007
Resistance to repeated warm/cool action (appearance)--clearKS F 4715 : 2007
Resistance to repeated warm/cool action (adhesive strength)N/㎟-0.8KS F 4715 : 2007
Water absorption coefficientkg/㎡h0.5-0.1KS F 4715 : 2007
Washability--clearKS F 4715 : 2007
Impact resistance--clearKS F 4715 : 2007
Alkali resistance--clearKS F 4715 : 2007
Weather resistance (appearance)--clearKS F 4715 : 2007
Weather resistance (discoloration)number-4KS F 4715 : 2007
Moisture permeability (sd)M-0.5KS F 4715 : 2007

Precautions

– Excessive water costs degrade the quality, so please observe the proper water ratio. 
– Construction in too hot weather may cause skin dryness, so please shade and refrain from construction.
– Work temperature above 5℃ and below 35℃, and install after proper maintenance of direct sunlight and wind as the cause of cracks.
– Please refrain from installing in rainy seasons or very humid days (over 85%).

Construction site utilization

Construction site utilization

CategoryAlseco SystemExposed concrete
(panel)
ZincDry BeatEnamelAL SHEETGranite
Structure
NonflammableNonflammable
(nonflammable)
Nonflammable
(nonflammable)
Nonflammable
(nonflammable)
Semi-incombustible
(flame retardant)
Nonflammable
(nonflammable)
Semi-incombustible
(flame retardant)
Nonflammable
(nonflammable)
ShockproofmiddleMiddle-lowTopmiddleTopTopMiddle-low
AdvantagesIn case of fire, it has toxic gas and environmental stability, and reinforces pollution resistance and waterproof performance.
Various colors available for remodeling or construction in new buildings
Expressing the strength and profoundness of concrete structures Ensure maintenance and durability Currently used in many buildingsYou can feel the sophisticated architectural beauty of the protruding joint method Applicable to walls and roofs in various colors Panel that is resistant to pollution and has a modern senseExcellent constructability and economy Apply various colors Apply to many buildings Applicable to remodeling and new buildingsShorten construction time due to excellent workability Great insulation effect when attaching rear insulation Various colors and aesthetics are applied to high-end buildingsShorten construction time due to excellent workability Great insulation effect when attaching rear insulation Various colors and aesthetics are applied to high-end buildingsExcellent durability, dignity in natural colors, and an image of a luxurious building
DisadvantagesGerman patented product, construction dependent on importSelf-load borne on the building Discoloration and contamination by whitening phenomenon and period Difficult to finish a single material due to lack of variety of materialsIf paint peels off due to external impact or careless construction, there is a risk of corrosion.
If construction is wrong, flatness cannot be guaranteed Vulnerable to external shock
When the seal passes due to bond bonding, the peeling phenomenon is severe and the problem of waterproofing occurs.
Vulnerable to fire by using ESP (Styrofoam).
Precise construction is required, and discoloration and fullness due to temperature change. After a certain period of time, a waterproof problem occurs at the joint (caulking).Precise construction is required, discoloration and fullness due to temperature change After a certain period of time, a waterproof problem occurs in the joint (caulking) part.Due to the nature of stone, it is burdened on the building due to its own load Whitening phenomenon due to deterioration of stone The construction period is long.
Scroll to Top